| Titre:  | Effect of H2O Content on Structure and Optical Properties of TiO2 Thin Films Derived by Sol-Gel Dip-Coating Process at Low Temperature |  
| Auteur(s):  | Kermadi, Salim Agoudjil, N. Sali, S. Tala-Ighil, Razika |  
| Mots-clés:  | TiO2 thin films Sol-gel Structural properties Optical properties |  
| Date de publication:  | 2008 |  
| Collection/Numéro:  | Chemical Physics Research Journal, Vol 2, Issue 3/4 ; 2008; |  
| Résumé:  | Pure TiO2 thin films were prepared on the glass substrates by sol–gel dip coating technique 
with titanium (IV) isopropoxide including simultaneously acetylacetone and acetic acid as 
stabilizing reagents. The effect of the amount of water in the sol on structural and optical 
properties of TiO2 thin films was investigated. The structural and optical properties of post-
sintered films for 1 hour at 500°C  in air were investigated  By X-ray diffraction (XRD), 
scanning electron microscopy (SEM), UV–Vis spectroscopy and ellipsometry. The results 
showed a simultaneous appearance of the rutile and the anatase phases with different rutile / 
anatase proportions for all samples. The increase of the water content leads to the decrease of 
rutile / anatase proportion. The crystalline size varies from 7.94 to 24.84 nm for the anatase 
phase and from 17.70 to 22.31 nm for the rutile phase. The optical measurements showed that 
the structure was strongly influenced by the water / alcoxides molar ratios. In comparison 
with the bulk material, the TiO2 thin films prepared by this way exhibit low refractive index in 
the range of 2.15 and high band gap energy narrowing from 3.88 to 3.95 eV for direct allowed 
transition and from 3.09 to 3.39 eV for indirect allowed transition according to the cristallinity 
degree and the rutile /anatase weight fraction. |  
| URI/URL:  | http://dlibrary.univ-boumerdes.dz:8080/handle/123456789/6448 |  
| ISSN:  | 0021-9606 |  
| Collection(s) : | Publications Internationales
  |  
  
Fichier(s) constituant ce document : 
Il n'y a pas de fichiers associés à ce document. 
 |   
    
    
     
    
    
    Tous les documents dans DSpace sont protégés par copyright, avec tous droits réservés. 
                    
                      
                 |